3M 1838

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

3M 1838

Main features

  • Controlled-Flow Structural Bonding
  • One-Hour Positioning Window
  • Rigid High-Shear Performance

Product Description

3M Scotch-Weld Epoxy Adhesive 1838 B/A Green is a green, two-part, room-temperature-curing structural epoxy with controlled flow for precise placement on metals, wood, and selected plastics. Part B and Part A mix at 4:5 by volume or 1:1 by weight, producing a uniform green material with a typical 60-minute open time and 60-minute work life for a 100 g mass at 23 deg C. The high-viscosity formulation limits movement after dispensing and cures to a rigid bond with high shear strength and environmental resistance. It is suited to structural assembly where accurate application, extended positioning time, and a firm cured bond are required.

Key features

  • Controlled-flow placement: High component viscosity limits movement and supports precise dispensing on the bond area.
  • Defined two-part ratios: Part B and Part A mix at 4:5 by volume or 1:1 by weight.
  • Extended positioning time: Typical open time and 100 g mixed work life are each 60 minutes at the stated conditions.

Applications

Applications include structural bonding of metals, wood, and selected plastics where controlled flow, room-temperature cure, and extended positioning time are required.

Product Family

3M 1838

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
White / Green
Component System
Two (Accelerator / Resin)
Mix Ratio
1:1
Physical Properties
Open time
60 minutes
Mechanical Properties
Elongation
2-3 %
Thermal Properties
Glass Transition Temperature (Tg)
55 °C
Thermal Conductivity
0.3 W/m.K
Electrical Properties
Volume Resistivity
ASTM D257 Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Component properties and mixed-material handling values remain separated; mix ratios retain their stated basis.

PropertyValueUnitMethod / condition
Mix ratio by volume (B:A)4:5-Before application
Mix ratio by weight (B:A)1:1-Before application
Base resinModified epoxy-Part A
Accelerator resinPolyamide-Part B
Base viscosity70,000 to 600,000cPPart A at 27 deg C
Accelerator viscosity300,000 to 1,000,000cPPart B at 27 deg C
Open time60minTypical mixed material
Work life60min100 g mixed at 23 deg C
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Cured colorGreen-Typical
Modulus344,000psiTypical at 23 deg C
Shore D hardness82-ASTM D2240 at 23 deg C
T-peel adhesion4lb/in widthASTM D1876; aluminum at 23 deg C
Elongation at break2 to 3%Typical
Tensile strength at break4,290psiTypical
Glass transition temperature55deg CMidpoint; DSC second heat at 20 deg C/min
Volume resistivity1.5 x 10^15ohm-cmASTM D257 at 23 deg C