3M 130C

Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 130C

Main features

  • Self-Fusing Linerless Insulation
  • High Dielectric Strength
  • 69 kV Splicing Scope

Product Description

Scotch Linerless Rubber Splicing Tape 130C is a black, linerless self-fusing EPR rubber splicing tape for primary insulation in cable splice and termination work. Its 0.76 +/- 0.076 mm construction combines an ethylene-propylene rubber backing with a fusible adhesive interlayer and is applied in highly stretched, half-lapped layers to build a uniform winding. The tape is rated for 90 deg C operation and 130 deg C emergency overload, with minimum dielectric strength of 27.6 kV/mm under ASTM D4325 test conditions. It is used for supported outdoor and underground electrical connections, including installations up to 69 kV when the specified application method and system conditions are met.

Key features

  • Self-fusing EPR construction: The linerless backing and fusible interlayer combine under stretch to build a uniform insulating wrap.
  • Electrical insulation performance: Minimum dielectric strength is 700 V/mil (27.6 kV/mm) under the stated ASTM D4325 condition.
  • Defined temperature ratings: The tape is rated for 90 deg C operation and 130 deg C emergency overload under ASTM D4388 Type III.

Applications

Applications include primary insulation for cable splices and terminations, plus supported outdoor and underground electrical connections in installations up to 69 kV.

Product Family

3M 130C

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black
Thickness range
0.76 +/- 0.076 mm
Thermal Properties
Thermal Conductivity
0.3 W/m.K
Mechanical Properties
Elongation
700 %
Electrical Properties
Dielectric Strength
27.6 kV/mm
Volume Resistivity
10¹⁴ Ohms⋅cm

Additional Information

Technical properties

As-supplied / before-processing properties

Properties are measured at 23 deg C unless the method / condition states otherwise.

PropertyValueUnitMethod / condition
ColorBlack-Visual
BackingEthylene-propylene rubber (EPR)-As supplied
Total thickness30 +/- 3 mil (0.76 +/- 0.076 mm)-ASTM D4325 at 23 deg C
Tensile strength250 (1.7)psi (MPa)Minimum; ASTM D4325 at 23 deg C
Elongation700%Minimum; ASTM D4325 at 23 deg C
Thermal conductivity0.3W/m-KNominal; ASTM C518 at 23 deg C
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Operating temperature rating90deg CASTM D4388 Type III
Emergency overload rating130deg CASTM D4388 Type III
Fusion at 300% strainPass-ASTM D4325
Dielectric strength700 V/mil (27.6 kV/mm); at least 90% after humidity-Minimum; standard and after 96 h at 23 deg C / 96% RH
Heat resistancePass-7 days at 130 deg C; ASTM D4325
Volume resistivity1 x 10^14 / 1 x 10^13ohm-cmMinimum after 96 h at 23 deg C / 50% RH and 96% RH
Ozone resistancePass-ASTM D4325
UV resistancePass-ASTM D4325