Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other

3M 1205

Main features

  • 155 deg C Continuous Operation
  • 6000 V Dielectric Minimum
  • Coil and Solder-Mask Versatility

Product Description

3M Polyimide Film Electrical Tape 1205 is an amber, 0.081 mm polyimide tape with a non-corrosive acrylic pressure-sensitive adhesive for electrical insulation and solder masking. Its 0.025 mm film backing provides a thin insulating construction for coils, capacitors, transformers, wire harnesses, lead anchoring, and printed circuit board assembly. The tape is designed for continuous operation not exceeding 155 deg C under its UL listing. ASTM D1000 values include minimum dielectric breakdown of 6000 V, minimum insulation resistance of 1 x 10^12 ohm, and minimum elongation of 50%, with properties measured at 23 deg C unless otherwise stated.

Key features

  • 155 deg C operation: The tape is designed for continuous operation not exceeding 155 deg C under its UL listing.
  • 6000 V dielectric minimum: ASTM D1000 dielectric breakdown is at least 6000 V at 23 deg C.
  • Pressure-sensitive installation: The acrylic adhesive requires no heat, moisture, or solvent preparation for application.

Applications

Applications include wrapping coils, capacitors, transformers, and wire harnesses; anchoring leads; and solder masking during printed circuit board assembly.

Product Family

3M 1205

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Acrylic
Color
Amber
Film Thickness
0.025 mm
Total Thickness
81 μm
Mechanical Properties
Adhesion Strength
20 Oz/in
Elongation
50 %
Electrical Properties
Breakdown Voltage
6000 V

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorAmber-Visual
BackingPolyimide film-As supplied
AdhesiveAcrylic-Non-corrosive pressure-sensitive adhesive
Backing thickness1 / 0.025mil / mmNominal
Total thickness3.2 +/- 0.5 / 0.081 +/- 0.013mil / mmASTM D1000 at 23 deg C
Shelf life5yearsFrom manufacture; 10 to 27 deg C and less than 75% RH
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Continuous operating temperature155deg CMaximum under UL listing
Dielectric breakdown6000VMinimum; ASTM D1000 at 23 deg C
Insulation resistance1 x 10^12ohmMinimum; ASTM D1000 at 23 deg C
Electrolytic corrosion factor1.0-3M ETM-54001; 1.0 equals no observed corrosion
Adhesion to steel20 / 2.2oz/in / N/cmMinimum; ASTM D1000 at 23 deg C
Breaking strength20 / 35lb/in / N/cmMinimum; ASTM D1000 at 23 deg C
Elongation50%Minimum; ASTM D1000 at 23 deg C
Flame retardancyPass-UL 510A