3M 1181

Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.

3M 1181

Main features

  • Conductive Adhesive Path
  • 66 dB Average Shielding
  • Solderable Die-Cut Construction

Product Description

3M EMI Copper Foil Shielding Tape 1181 is a 0.066 mm copper foil tape with an electrically conductive acrylic pressure-sensitive adhesive and removable liner for EMI/RFI shielding and static charge control. Silver-coated glass beads in the adhesive create an electrical path between the copper backing and the application surface. The tape averages 66 dB shielding effectiveness from 300 kHz to 2.5 GHz under ASTM D4935 testing and has maximum electrical resistance of 0.005 ohm/in2 under the stated MIL-STD-202 test. It can be die-cut and soldered for shielded-room seams, cable wrapping, electrical contact to non-solderable surfaces, and prototype electronics work.

Key features

  • Conductive adhesive path: Silver-coated glass beads provide electrical continuity between the flat copper foil and application surface.
  • Measured shielding performance: Average shielding effectiveness is 66 dB from 300 kHz to 2.5 GHz under ASTM D4935.
  • Fabrication versatility: The lined copper tape can be die-cut and soldered for production or prototype configurations.

Applications

Applications include EMI/RFI shielding, static charge draining, seaming shielded rooms, cable wrapping, contact to non-solderable surfaces, die-cut components, prototyping, and troubleshooting.

Product Family

3M 1181

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer
Electrically Conductive Acrylic
Color
Copper
Film Thickness
0.036 mm
Total Thickness
66.04 μm
Mechanical Properties
Adhesion Strength
25 Oz/in

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorCopper-Visual
BackingFlat copper foil-As supplied
AdhesiveElectrically conductive acrylic-Pressure-sensitive adhesive
Backing thickness1.4 / 0.036mil / mmNominal
Total thickness2.6 +/- 0.2 / 0.066 +/- 0.005mil / mmASTM D1000 at 23 deg C
Shelf life5yearsFrom manufacture; 10 to 27 deg C and less than 75% RH
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Electrical resistance0.005ohm/in2Maximum; MIL-STD-202 Method 307 at 5 psi over 1 in2
Shielding effectiveness66dBAverage; ASTM D4935, 300 kHz to 2.5 GHz at 23 deg C
Adhesion to steel25 / 2.7oz/in / N/cmMinimum; ASTM D1000 at 23 deg C
Breaking strength22 / 39lb/in / N/cmMinimum; ASTM D1000 at 23 deg C
Flame retardancyPass-UL 510A, Category OARC2, File E17385