3M™ Nitrile High Performance Plastic Adhesive 1099 is a fast-drying, medium-viscosity nitrile rubber adhesive designed for brush or flow applications. It cures to form strong, flexible bonds that resist weathering, water, fuels, oil, and plasticizers. This high-performance adhesive can be used at room temperature or heat-cured to obtain superior physical properties, making it highly versatile for various assembly needs.

Key features

  • Fast drying: Rapidly forms strong, flexible bonds to help accelerate production and assembly processes.
  • Exceptional resistance: Delivers robust durability against weathering, water, fuels, oil, and plasticizers.
  • Heat-cure option: May be cured with heat to achieve superior physical and mechanical properties.

Applications / Suitable for

  • Bonding vinyl extrusions and sheeting
  • Adhering fabrics, foams, and many plastics
  • Industrial brush or flow applications
Product Family

3M 1099

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance
Light Tan
Density (g)
part A: 1.00/ part B: 1.15 g/cm3
Solids
31-37 %
Thermal Properties
Flash Point
-15 °C
Mechanical Properties
Peel Strength
29 N/cm

Additional Information

Technical properties

As-supplied / before-processing properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
Base Nitrile Rubber - -
Color Light Tan - Wet and dry
Solids Content by Weight 31-37 % -
Carrier Solvent Acetone - -
Viscosity 2000-4000 cP at 27°C (80°F)
Flash Point -15 °C Closed Cup
Bonding Range Up to 40 minutes -
Technical properties

After-processing / final-state properties

Typical properties; these values are not intended for use in preparing specifications.

Property Value Unit Method / condition
180° Peel Adhesion 29 N/cm Canvas to Steel, 24h at 23°C (73°F)
45 N/cm Canvas to Steel, 72 h at 23°C (73°F)
48 N/cm Canvas to Steel, 168 h at 23°C (73°F)
54 N/cm Canvas to Steel, 14 days at 23°C (73°F)
31 N/cm Canvas to Steel, 21 days at -34°C (29°F)
12 N/cm Canvas to Steel, 21 days at 66°C (150°F)
Overlap Shear Strength

3.2 MPa Aluminum to Aluminum, 121°C cure
21 MPa Aluminum to Aluminum, 177°C cure, tested at -55°C
9.0 MPa Aluminum to Aluminum, 177°C cure, tested at 23°C
6.2 MPa Aluminum to Aluminum, 177°C cure, tested at 66°C