3M 08463

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

3M 08463

Main features

  • One-Hour Full Cure
  • Closed-Cell Cavity Filling
  • Direct Static-Mix Application

Product Description

3M Flexible Foam 08463 is a two-part urethane foam-in-place system for replacing flexible OEM foam in vehicle body cavities. The mixed liquid is dispensed through a static mixing nozzle and develops into a closed-cell, 100% solids foam. A typical full cure is one hour at 23 deg C, and unrestricted foam density is 0.13 kg/L. The flexible cured material provides insulation and sound-deadening functions in enclosed automotive structures, giving collision-repair technicians a direct-application material for restoring foam in door intrusion beams, roof bows, body-side panels, and other NVH cavities after welding is complete. It is supplied in a 200 mL dual cartridge for compatible static-mix application.

Key features

  • Static-mix dispensing: The dual cartridge combines both urethane components through a static mixing nozzle for direct cavity application.
  • Closed-cell 100% solids: The cured closed-cell foam provides insulation and sound-deadening functions without a solvent-bearing formulation.
  • One-hour full cure: The mixed foam reaches a typical full cure in one hour at 23 deg C.

Applications

Applications include replacement of flexible OEM foam in door intrusion beams, roof bows, body-side panels, and other closed vehicle cavities used for NVH reduction, insulation, or sound deadening.

Product Family

3M 08463

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color
Black | Amber/Brown
Component System
Two Part (Urethane | Curative )
Solids
100 %
Thermal Properties
Flash Point
>149 °C
Service temperature
-20 to 82 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values apply to the 200 mL two-part cartridge before mixing unless stated otherwise.

PropertyValueUnitMethod / condition
ComponentsUrethane base and curative-Two-part system before mixing
Component colorsBlack and amber / brown-Before mixing
Flash pointGreater than 149deg CTypical
Solids content100%Typical
ConsistencyLiquid-Before mixing
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
Service temperature-20 to 82deg CCured foam; typical
Foam density0.13kg/LUnrestricted foam; typical
Full cure time1hTypical at 23 deg C ambient and substrate temperature

Leading Brands Trust in Our Products and Services